  4. Hardened and Softened Insulation Are Two Opposite Aging Modes: Whether the Plasticiser Leaves or Enters Decides Which Number You Measure

Hardened and Softened Insulation Are Two Opposite Aging Modes: Whether the Plasticiser Leaves or Enters Decides Which Number You Measure

Key takeaways

Insulation aging is not a single direction. When plasticiser and small molecules leave, the compound hardens and cracks; when media enter, or the crosslink is underdeveloped, it softens, turns tacky and shrinks back. The criteria differ too: tensile strength can rise before it falls, elongation drops first, so strength alone lets a brittle part pass, and insulation resistance or withstand voltage often still pass while the compound is brittle. Sampling must include the crimp zone, the bend and the section next to heat sources, otherwise the locations where failures actually occur sit outside the criterion.

"The harness is gone" covers two opposite failures. In one, the insulation is brittle enough to snap when bent; in the other it is tacky, soft, and has shrunk back from the terminal leaving a short length of bare conductor. The first is plasticiser and small molecules leaving the compound. The second is media getting in, or a crosslink that never developed. The number you measure and the step you change are not the same in the two cases.

Both can also pass an electrical test without any visible sign.

This piece covers the insulation body only. Abrasion is mechanical wear, covered in harness vibration testing; cracking driven by structure plus media is covered in stress cracking in plastics; shrinkage of a seal after media extraction is covered in compression set and media compatibility of seals. Sampling positions and criteria differ across all three, and mixing them produces wrong conclusions.

1. Separate hardened from softened

Insulation is not a single material. On the same harness, PVC, cross-linked polyolefin, silicone rubber and thermoplastic elastomer age along different paths, and the visible direction can reverse.

Insulation materialDominant aging pathDirectionWhat you see on the harness
------------
PVCPlasticiser loss by volatilisation and migration, dehydrochlorinationHardens and embrittles first, may turn tacky laterFine cracks on bending, whitened fracture, stiff end near the terminal
Cross-linked polyolefinOxidative chain scission, copper-catalysed degradation, water treesEmbrittles, locally powdersPowdering when stripped, abnormal discolouration of the conductor
Silicone rubberMigration of small molecules from incomplete cure, high-temperature cleavageEither direction is possibleTacky dust-attracting surface, slow rebound
Thermoplastic elastomerSoft-segment oxidation, swelling in oilsMostly softening and saggingSwollen section at oil contact, drop in peel force

Hardening usually means something left the compound; softening usually means something entered it, or the compound was never cured far enough.

Those two sentences cover most shop-floor judgement calls. The exceptions need the sampling position and the contact media to settle: silicone softening often traces to incomplete cure rather than any medium, while PVC from which a medium has extracted plasticiser shrinks and hardens, which reads like faster aging than it is.

Hardening is also not uniform. The crimp zone near the terminal, the run next to a heat source or bundled against another hot circuit, and the tight bend radius always go first. Cutting a section from the middle of the run and finding it normal often only proves the middle has not reached that stage yet.

2. The criterion is not "it still looks fine"

Insulation aging is quiet on electrical measurements. Insulation resistance and withstand voltage commonly still pass while the compound is brittle, because no crack has bridged and creepage distance has not yet shrunk to a problem. An electrical pass therefore does not replace a mechanical criterion, and visual inspection does not either, since tackiness and shrink-back are easily written off as assembly issues.

CriterionWhat it answersWhat it misses
---------
Tensile strength retentionHow much load capacity remainsThe early stage, where strength can rise before it falls
Elongation at break retentionWhether it can still bend and absorb deformationOnly meaningful against unaged parts of the same lot
Insulation resistance and withstand voltageWhether current leaks nowBrittleness, tackiness and shrink-back that have not bridged
Visual check and cross-sectionCracks, powdering, shrink-backDepends heavily on sampling position and reader experience

Elongation falls before tensile strength.

While plasticiser is only starting to leave, the compound stiffens and the strength reading can sit above a new part; once it truly embrittles, strength drops quickly. Measuring strength alone, or at a single point in time, returns a pass across exactly that window.

Retention must be referenced to unaged parts from the same lot, not to the catalogue typical value. The catalogue figure is a typical value at delivery and lots already scatter around it, so comparing an aged part against it folds lot variation into the aging number. The same logic is laid out in why data before and after a test do not agree.

3. Three accelerators beyond chamber temperature

Insulation temperature is not chamber temperature. A conductor carrying current heats itself, so a loaded run and an unloaded run expose the insulation to different temperatures; because aging is exponentially sensitive to temperature, that gap grows over time. Whether the run is loaded is therefore part of the condition, not an optional detail.

AcceleratorHow it actsWhat the plan must state
---------
Conductor self-heatingInsulation runs hotter than the chamberLoad current and energisation mode, or explicitly unloaded
Bending and fixingResidual stress at the bend adds to agingBend radius, fixing points, routing
Media contactExtraction or swelling by oil, coolant, cleanerMedia name and contact mode
Crimp zoneLocal stress plus copper-catalysed oxidationWhether sampling includes the crimp

Media contact is where plans get vague. "It has seen engine oil" and "immersed in a specified medium at a specified temperature" are different conditions with different criteria. Reagent families and contact conditions are written per chemical load in GB/T 28046.5 and are not repeated here.

On extrapolating duration: extending time at one temperature, or shortening it at a higher temperature, requires proof that the failure mechanism has not changed. Once the mechanism shifts, for example from plasticiser migration to oxidative scission, extrapolation no longer holds. That is set out in what a test duration can represent; here one line is enough: extrapolation rests on an unchanged mechanism, not on a good curve fit.

4. Why the terminal end fails first

Two causes overlap.

The first is shrink-back. Under heat history and crimp stress the compound relaxes, the end retreats and a short length of conductor is exposed, reducing creepage distance and bend allowance together. The second is copper catalysis: copper ions accelerate oxidation of polyolefin insulation, and the crimp zone is exactly where stress concentrates, so both conditions meet in the same short length.

Shrink-back is not a short crimp; it is the compound relaxing under temperature and stress.

Measure it after the same temperature history has been applied, not on a part straight off the line, where relaxation is still incomplete.

The practical consequence is sampling position. A plan that says "take one section from the middle of the run" places the crimp zone, the bend and the heat-adjacent run outside the criterion entirely. The link between part count and sampling points is covered in sample quantity and how representative a verdict is.

5. Five columns the test plan must fill

ColumnWhat to stateWhat it costs when omitted
---------
Temperature class and loadingLimits, dwell, transition; load current and energisationInsulation temperature differs from chamber temperature, results not comparable
Specimen state and routingBend radius, fixing points, whether the crimp is includedThe locations that actually fail sit outside the criterion
Media contactMedia name, contact mode, temperature"It has seen oil" cannot be reproduced
Criteria and retention basisWhich items, compared against which parts, at which positionsComparing to catalogue values turns lot variation into aging
Sampling and part countHow many positions per section, how destructive items are countedDestructive items consume the parts later items need

Of the five, media contact and the retention basis are the two most often merged into "per the standard". But GB/T 28046 and ISO 16750 supply application conditions and judgement grades; they do not know your routing, which medium the run touches, or where the crimp sits. Those come from the technical agreement. Criteria for the insulation body and its sampling rules usually live in the material specification and the customer agreement, which is the order the request form on the materials and component testing side should follow.

A few plain words

  • Decide the direction first, then the conditions. Hardening sends you to formulation and temperature history; softening sends you to media and cure state. The corrective actions point in opposite directions.
  • An electrical pass is not proof the insulation has not aged. By the time elongation has dropped, insulation resistance commonly still looks good.
  • A single strength reading is easily fooled by the rise-then-fall pattern. Measure retention, against unaged parts from the same lot.
  • Sample the crimp zone, the bend and the heat-adjacent run separately. Mid-run data does not answer questions about those places.
  • Write the full media list: coolant, brake fluid, washer fluid, cleaner and urea sit alongside engine oil.
  • TMC LAB confirms sampling positions and the media list before discussing condition grades on harness programmes, because the reverse order makes later results hard to attribute.

Scheduling is arranged per project; you can state your expected delivery date when submitting samples, and we will confirm a feasible plan against the current schedule and report progress at each milestone.

Related Q&A

Related questions

Frequently asked questions on the same topic. The first paragraph of each answer is the conclusion.

The insulation snaps when bent - is the compound simply not temperature resistant?
Separate the direction before discussing temperature. Snapping means the compound has embrittled, and the usual paths are plasticiser loss through volatilisation and migration, oxidative chain scission, and copper-catalysed degradation of polyolefin insulation, with temperature acting as one accelerator among them. Two things decide the judgement: how far elongation at break has dropped, and where the embrittlement is concentrated. If it appears only at the crimp and next to heat sources, suspect local temperature and stress; if the whole run is uniformly brittle, a formulation or incoming-lot issue is more likely. Temperature class comes from the applicable standard and the customer technical agreement, not from how a snapped sample felt.
Insulation resistance and withstand voltage both pass - does that prove the insulation has not aged?
It does not. Those two tests answer whether current leaks now, and they are insensitive to degradation that has not yet bridged: a compound can be brittle, the surface tacky and the end shrunk back, and both readings remain normal as long as no conductive path has formed. The early signal of insulation aging is mechanical - elongation at break falls first, while tensile strength may rise before it falls. Judge on mechanical retention with electrical results as support, and compare against unaged parts from the same lot rather than against the catalogue typical value.
A short length of conductor is exposed at the terminal - is that assembly or material?
It is usually insulation shrink-back from relaxation under heat history and stress, not a crimp that was made too short. The consequence is not cosmetic: exposed conductor reduces creepage distance and eats into bend allowance at the same time. Measure shrink-back after the same temperature history has been applied - a part straight off the line has not finished relaxing and will read low. Then split by cause: overall relaxation points back to compound and temperature class, while shrink-back confined to the crimp zone points first at crimping process and terminal choice.

These answers share the same data source as the FAQ page.

Have a testing requirement? Send us your product details

Tell us the product model and test requirements. Our engineers will map out the test plan, the applicable standards and the item combination, and provide a quotation reference. The more specific the request, the sharper the answer.

  • Free scoping of the test plan and standards
  • Pre-scan testing during R&D to cut rework cost
  • On-site visits and witnessed testing supported
  • Scheduling per project, with progress updates at each milestone

Received — we will contact you shortly and follow up with a test plan and quotation.

By submitting you agree to be contacted by phone or email. Scheduling follows the project’s actual availability and is subject to mutual confirmation.

13510907826
Call